Chemical bath deposition (CBD) was used to grow ZnO nanorods on glass substrates. Grown ZnO nanorods are dipped in a copper nitrate trihydrate [Cu(NO 3) 2.3 H 2 O] solution at 90 °C for 30 min before being annealed at 400 °C for 1 h to convert Cu 2+ ions to CuO nanoparticles, forming a ZnO/CuO thin films nanocomposite. Images obtained from a Field …